Chemical properties
Property | Value |
---|---|
Aluminio | 2 - 3 % Show Material materials with Aluminio of 2 - 3 % |
Cobre | 58 - 60 % Show Material materials with Cobre of 58 - 60 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 - 0.7 % Show Material materials with Hierro of 0.3 - 0.7 % |
Manganeso | 3 - 4 % Show Material materials with Manganeso of 3 - 4 % |
Níquel | 0.3 - 0.5 % Show Material materials with Níquel of 0.3 - 0.5 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |