Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 2E-3 % Show Material materials with Arsénico of 2E-3 % |
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 2E-3 % Show Material materials with Carbono of 2E-3 % |
Fósforo | 2E-3 % Show Material materials with Fósforo of 2E-3 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Níquel | 0.52 - 0.58 % Show Material materials with Níquel of 0.52 - 0.58 % |
Otro | Rest Cu, total 0.10 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 2E-3 % Show Material materials with Silicona of 2E-3 % |