Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 95 - 98 GPa Show Material materials with Módulo elástico of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 2E-3 % Show Material materials with Arsénico of 2E-3 % |
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 2E-3 % Show Material materials with Carbono of 2E-3 % |
Fósforo | 2E-3 % Show Material materials with Fósforo of 2E-3 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Níquel | 0.57 - 0.63 % Show Material materials with Níquel of 0.57 - 0.63 % |
Otro | Rest Cu, total 0.10 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 2E-3 % Show Material materials with Silicona of 2E-3 % |