General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Arsénico | 0.01 % Show Material materials with Arsénico of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 1 - 1.4 % Show Material materials with Hierro of 1 - 1.4 % |
Manganeso | 0.3 - 0.8 % Show Material materials with Manganeso of 0.3 - 0.8 % |
Níquel | 5 - 6.5 % Show Material materials with Níquel of 5 - 6.5 % |
Otro | Rest Cu, total 0.7 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |