Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 0.1 % Show Material materials with Azufre of 0.1 % |
Estaño | 11.2 - 13 % Show Material materials with Estaño of 11.2 - 13 % |
Fósforo | 0.25 - 0.6 % Show Material materials with Fósforo of 0.25 - 0.6 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Cu, total 0.20 |
Plomo | 0.5 % Show Material materials with Plomo of 0.5 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |