Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Magnesio | 0.7 - 0.85 % Show Material materials with Magnesio of 0.7 - 0.85 % |
Níquel | 6E-3 % Show Material materials with Níquel of 6E-3 % |
Otro | Rest Cu, total 0.3 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Zinc | 5E-3 % Show Material materials with Zinc of 5E-3 % |