Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 75 [-] Show Supplier Material materials with Dureza Brinell of 75 [-] |
Elongación A5 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A5 of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 195 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 195 MPa |
Resistencia a la tracción | 23.0 °C | 245 MPa Show Supplier Material materials with Resistencia a la tracción of 245 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | balance |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.05 % Show Supplier Material materials with Cromo of 0.05 % |
Hierro | 0.1 - 0.3 % Show Supplier Material materials with Hierro of 0.1 - 0.3 % |
Magnesio | 0.35 - 0.6 % Show Supplier Material materials with Magnesio of 0.35 - 0.6 % |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.3 - 0.6 % Show Supplier Material materials with Silicona of 0.3 - 0.6 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.15 % Show Supplier Material materials with Zinc of 0.15 % |
Technological properties
Property | ||
---|---|---|
Coating | suitable for electro-chemical brightening and anodizing, for high decorative demands | |
Corrosion properties | corrosion resistant | |
Processing methods | excellent forming properties | |
Welding | weldable |