Chemical properties
Property | Value |
---|---|
Aluminio | balance |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % |
Magnesio | 0.4 - 0.6 % Show Supplier Material materials with Magnesio of 0.4 - 0.6 % |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.6 - 0.9 % Show Supplier Material materials with Silicona of 0.6 - 0.9 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |