General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 23.0 °C | 7.21 g/cm³ Show Supplier Material materials with Densidad aparente of 7.21 g/cm³ | |
Tamaño de partícula | 40 - 100 nm Show Supplier Material materials with Tamaño de partícula of 40 - 100 nm | BET | |
Área superficial específica | 8 - 20 m²/g Show Supplier Material materials with Área superficial específica of 8 - 20 m²/g | BET |
Technological properties
Property | ||
---|---|---|
Application areas | ceramic membranes, barrier layer SOFC, SOFC, solid oxide fuel cell, oxygen separation membranes, solid electrolyte, electronic conductor, membrane reactor, oxygen ionic transport membrane, dual-phase membrane, hydrogen separation membrane, cathode SOFC, protective layer SOFC, oxygen sensor | |
Chemical composition | Ce0.9Gd0.1O2-δ | |
Color | Fine, pale yellow powder | |
Crystal structure | Crystal structure at 25°C: Cubic flourite, Fm-3m | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |