General
Property | Value | Comment |
---|---|---|
Tamaño de partícula | 35 - 100 nm Show Supplier Material materials with Tamaño de partícula of 35 - 100 nm | BET |
Área superficial específica | 10 - 25 m²/g Show Supplier Material materials with Área superficial específica of 10 - 25 m²/g |
Technological properties
Property | ||
---|---|---|
Application areas | solid oxide fuel cell, SOFC, cathode, electrode, catalyst, ceramic membrane. | |
Chemical composition | (La0.8Sr0.2)0.99MnO3-δ | |
Color | Fine, black powder | |
Crystal structure | Crystal structure at 25°C: Rhombohedral perovskite, R-3c | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |