General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.91 - 0.92 g/cm³ Show Supplier Material materials with Densidad of 0.91 - 0.92 g/cm³ | GOST 15139 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 88 - 92 [-] Show Supplier Material materials with Dureza Shore A of 88 - 92 [-] | GOST 24621 |
Elongación | 23.0 °C | 600 % Show Supplier Material materials with Elongación of 600 % | GOST IEC 60811-1-1 |
Resistencia a la tracción | 23.0 °C | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | GOST IEC 60811-1-1 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al aislamiento superficial | 23.0 °C | 1.00E+16 Ω·cm² Show Supplier Material materials with Resistencia al aislamiento superficial of 1.00E+16 Ω·cm² | Min., GOST 50499 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 3 - 9 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3 - 9 g/10min | GOST 11645, 190°С/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Flexible low-voltage power cables. | |
Processing methods | 1. Screw configuration: barrier screw, compression index of 2-2.5. Temperature profile: Zone 1: 135°С, Zone 2: 140°С, Zone 3: 155°С, Zone 4: 170°С, Die plate: 200-210°С. Screw thermostatic (if available) 85-90°С. 2. Crosslinking recommendations: Water temperature 90-95°С. The exposure time at the rate of 240 min (4 hours) per 1.0 mm of thickness. Metalen К-51 Thermal strain at 200°С: 40% and Percentage elongation: 0%. |