General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 - 0.965 g/cm³ Show Supplier Material materials with Densidad of 0.95 - 0.965 g/cm³ | ISO 1183/ISO 1872-2B |
Mecánica
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0.5 - 0.7 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 0.5 - 0.7 g/10min | ISO 1133, 190°С/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | METALEN PE-1 is recommended for the top coat of pipe insulation by side or circular (longitudinal) extrusion. | |
Processing methods | METALEN PE-1 is recommended to be processes on extruders with a flat or circular die. METALEN PE-1 ensures good processability in wide temperature range.The below conditions may be used when starting the extruder: Barrel: 190–230°C, Head: 190–230°C, Die: 220–225°C, Melt temperature: 220–225°C. Definitive processing recommendations may only be given when the specific material application and the equipment type used are known. |