Material: el 'Alloy 36 (Invar®) Controlled Expansion Alloy' que buscabas ha sido remplazado por el material siguiente.

Alloy 36 (Invar®) Controlled Expansion Alloy

View suppliers (21)
Want to keep this datasheet? Save it now in your required format

Description

1.3912 (FeNi36) is a 36% nickel-iron alloy. It exhibits a near zero rate of thermal expansion from around –100°C up to 200°C. This is around a tenth of the expansion rate of carbon steels. Alloy 36 also demonstrates a high retention of strength and toughness at cryogenic temperatures, making it suitable for a variety of low temperature or low expansion applications. The alloy is ideally suited to areas where dimensional changes due to temperature must be minimal, such as tooling for aerospace composites, radio and electronic devices and structural members in precision equipment such as lasers, measuring devices, thermostats and cryogenic instrumentation. Alloy 36 can also be utilised in combination with a high expansion material to crate mechanical movement with temperature in thermomechanical controls and switchgear.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

8.13 g/cm³

Show Material materials with Densidad of 8.13 g/cm³

Mecánica

PropertyTemperatureValue

Dureza Vickers

23.0 °C

140 [-]

Show Material materials with Dureza Vickers of 140 [-]

Elongación

23.0 °C

30 %

Show Material materials with Elongación of 30 %

Límite elástico

23.0 °C

310 MPa

Show Material materials with Límite elástico of 310 MPa

Módulo elástico

23.0 °C

140 GPa

Show Material materials with Módulo elástico of 140 GPa

Resistencia a la tracción

23.0 °C

480 MPa

Show Material materials with Resistencia a la tracción of 480 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

23.0 °C

510 J/(kg·K)

Show Material materials with Calor específico of 510 J/(kg·K)

Coeficiente de dilatación térmica

30.0 °C

1.2E-6 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.2E-6 1/K

150.0 °C

2.7E-6 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.7E-6 1/K

Conductividad térmica

23.0 °C

10.5 W/(m·K)

Show Material materials with Conductividad térmica of 10.5 W/(m·K)

Temperatura de fusión

1450 °C

Show Material materials with Temperatura de fusión of 1450 °C

Chemical properties

PropertyValue

Hierro

63 %

Show Material materials with Hierro of 63 %

Manganeso

0.6 %

Show Material materials with Manganeso of 0.6 %

Níquel

36 %

Show Material materials with Níquel of 36 %

Silicona

0.4 %

Show Material materials with Silicona of 0.4 %

Technological properties

Property
Application areas

General: Positioning devices, bimetal thermostats, advanced composite moulds for aerospace industry, optical devices, echo boxes and filters for mobile telephones, magnetic shielding, small electrical transformers, metrology devices, scientific instruments, electrical circuit breakers, temperature regulators, clock balance wheels, pendulum clocks, precision condenser blades, radar and microwave cavity resonators, special electronic housings, seals, spacers, and specialized frames, high voltage transmission lines