Chemical properties
Property | Value | Comment |
---|---|---|
Cobre | 99.95 % Show Material materials with Cobre of 99.95 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | General: Radar and other electronic equipment, anodes for vacuum tubes, glass to metal seals in electronic equipment, thermostatic control valves, rotor conductors for large generators and motors, electrical equipment for service at elevated temperatures in the presence of reducing gases and anodes for electroplating, particularly in cyanide baths |