2.1504 (CuNi14Al3) is an extra high strength copper nickel alloy developed by Columbia Metals that maximises both strength and corrosion resistance. Sometimes referred to as a nickel bronze, NIBRON® contains additions of aluminium, iron and manganese that join with the copper and nickel to achieve its exceptional properties. Although suited primarily to the tough extremes of marine or offshore oil and gas environments, Nibron® has also established itself for critical components in many other industrial sectors including aerospace, electrical, chemical and automotive. It shows the following features and properties:


  • Very high mechanical properties
  • Excellent wear and galling resistance
  • High ductility
  • Outstanding resistance to marine corrosion and erosion
  • Retention of properties at cryogenic temperatures
  • Exceptionally low magnetic permeability
  • Good machinability and dimensional stability
  • Good thermal conductivity
  • Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyTemperatureValue

    Densidad

    23.0 °C

    8.5 g/cm³

    Show Material materials with Densidad of 8.5 g/cm³

    Mecánica

    PropertyTemperatureValue

    Dureza Brinell

    23.0 °C

    229 - 240 [-]

    Show Material materials with Dureza Brinell of 229 - 240 [-]

    Elongación

    23.0 °C

    12 %

    Show Material materials with Elongación of 12 %

    Límite elástico Rp 0,2

    23.0 °C

    555 - 630 MPa

    Show Material materials with Límite elástico Rp 0,2 of 555 - 630 MPa

    Módulo elástico

    23.0 °C

    141 GPa

    Show Material materials with Módulo elástico of 141 GPa

    Resistencia a la tracción

    23.0 °C

    770 - 850 MPa

    Show Material materials with Resistencia a la tracción of 770 - 850 MPa

    Aplicaciones térmicas

    PropertyTemperatureValueComment

    Coeficiente de dilatación térmica

    23.0 °C

    1.64E-5 1/K

    Show Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K

    for 0-400°C

    Conductividad térmica

    23.0 °C

    44 - 46 W/(m·K)

    Show Material materials with Conductividad térmica of 44 - 46 W/(m·K)

    Temperatura de fusión

    1080 - 1100 °C

    Show Material materials with Temperatura de fusión of 1080 - 1100 °C

    Eléctrico

    PropertyTemperatureValue

    Resistividad eléctrica

    23.0 °C

    1.7E-7 Ω·m

    Show Material materials with Resistividad eléctrica of 1.7E-7 Ω·m

    Magnético

    PropertyTemperatureValueComment

    Permeabilidad magnética relativa

    23.0 °C

    1 [-]

    Show Material materials with Permeabilidad magnética relativa of 1 [-]

    max.

    Chemical properties

    PropertyValue

    Aluminio

    3 %

    Show Material materials with Aluminio of 3 %

    Cobre

    Balance

    Hierro

    1.5 %

    Show Material materials with Hierro of 1.5 %

    Manganeso

    0.3 %

    Show Material materials with Manganeso of 0.3 %

    Níquel

    14.5 %

    Show Material materials with Níquel of 14.5 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Marine shafts and bearing bushes, offshore bolting, valve and pump trim;Aerospace: Aircraft landing gear bushes, actuating sleeves, steering gear, bearing bushes, non-magnetic bolts and control surface components;Automotive: High performance engine shafts, gears, pinions, bearing bushes, locking nuts, mechanical and electromechanical components, thrust washers and hydraulic equipment;Chemical processing: Pump and valve spindles and other trim, flanges, pipe fittings, clamps and plant components

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Good machinability