General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.87 g/cm³ Show Material materials with Densidad of 8.87 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 155 - 180 [-] Show Material materials with Dureza Brinell of 155 - 180 [-] |
Elongación | 23.0 °C | 10 % Show Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 430 - 590 MPa Show Material materials with Límite elástico Rp 0,2 of 430 - 590 MPa |
Resistencia a la tracción | 23.0 °C | 550 - 640 MPa Show Material materials with Resistencia a la tracción of 550 - 640 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | for 0-400°C |
Conductividad térmica | 23.0 °C | 160 W/(m·K) Show Material materials with Conductividad térmica of 160 W/(m·K) | |
Temperatura de fusión | 1040 - 1060 °C Show Material materials with Temperatura de fusión of 1040 - 1060 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.03E+7 S/m Show Material materials with Conductividad eléctrica of 2.03E+7 S/m |
Specific Electrical conductivity | 35 % IACS Show Material materials with Specific Electrical conductivity of 35 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Níquel | 1.6 - 2.2 % Show Material materials with Níquel of 1.6 - 2.2 % |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive: Valve guides, valve seats, gears, rocker and little end bushes or internal combustion engines requiring extreme performance;Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Other: Non-magnetic instrument components and spark-resistant safety tooling | |
Cold Forming | It can be cold formed | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Easily machined | |
Hot forming | It can be hot formed |