General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 190 - 200 [-] Show Material materials with Dureza Brinell of 190 - 200 [-] |
Elongación | 23.0 °C | 10 % Show Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 570 - 750 MPa Show Material materials with Límite elástico Rp 0,2 of 570 - 750 MPa |
Resistencia a la tracción | 23.0 °C | 690 - 800 MPa Show Material materials with Resistencia a la tracción of 690 - 800 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | for 0-400°C |
Conductividad térmica | 23.0 °C | 159 W/(m·K) Show Material materials with Conductividad térmica of 159 W/(m·K) | |
Temperatura de fusión | 1060 - 1085 °C Show Material materials with Temperatura de fusión of 1060 - 1085 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.74E+7 S/m Show Material materials with Conductividad eléctrica of 1.74E+7 S/m |
Specific Electrical conductivity | 30 % IACS Show Material materials with Specific Electrical conductivity of 30 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Níquel | 2.6 - 4.5 % Show Material materials with Níquel of 2.6 - 4.5 % |
Silicona | 0.8 - 1.3 % Show Material materials with Silicona of 0.8 - 1.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive: valve guides, bushes and valve seats;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Offshore & marine: Downhole tools, shear pins, hydraulic valve bodies, pump components and ball valves and mechanical seals;Other: Non-magnetic tooling, plastic mould tooling, friction pads and fibre optic connectors | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Good machinability |