Tungsten alloys, which contain elements such as nickel, copper and iron, produce a host of alloys which have engineering properties similar to steel, are relatively easy to machine, and can be plated or painted to enhance their corrosion protection. These alloys are approximately 50% denser than lead resulting in a higher concentration of mass in a limited area.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

18 g/cm³

Show Material materials with Densidad of 18 g/cm³

Mecánica

PropertyTemperatureValue

Dureza Rockwell C

23.0 °C

34 [-]

Show Material materials with Dureza Rockwell C of 34 [-]

Elongación

23.0 °C

1 %

Show Material materials with Elongación of 1 %

Límite elástico

23.0 °C

517 MPa

Show Material materials with Límite elástico of 517 MPa

Módulo elástico

23.0 °C

345 GPa

Show Material materials with Módulo elástico of 345 GPa

Resistencia a la tracción

23.0 °C

648 MPa

Show Material materials with Resistencia a la tracción of 648 MPa

Chemical properties

PropertyValue

Wolframio

95 %

Show Material materials with Wolframio of 95 %

Technological properties

Property
Application areas