General
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | ISO 62 | 23 °C | 50 % r.h., Equilibrium | |
0.7 % Show Supplier Material materials with Absorción de agua of 0.7 % | ISO 62 | Water at 23 °C, Saturation | ||
Densidad | 25 °C | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | ISO 1183-1 | |
Low volatile organic compounds emissions | 23 °C | 10 μg/g Show Supplier Material materials with Low volatile organic compounds emissions of 10 μg/g | VDA 278 | max. |
Total volatile organic compounds emissions | 23 °C | 15 μgC/g Show Supplier Material materials with Total volatile organic compounds emissions of 15 μgC/g | VDA 277 | max. |
Volatile organic compounds emissions | 23 °C | 10 μg/g Show Supplier Material materials with Volatile organic compounds emissions of 10 μg/g | VDA 278 | max. |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 70 % Show Supplier Material materials with Elongación of 70 % | ISO 527-1/2 | 50 mm/min | |
Elongation at yield | 4.7 % Show Supplier Material materials with Elongation at yield of 4.7 % | ISO 527-1/2 | 50 mm/min | |
Límite elástico | 55 MPa Show Supplier Material materials with Límite elástico of 55 MPa | ISO 527-1/2 | 50 mm/min | |
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | |
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO 527-1/2 | 1 mm/min | |
Resistencia a la flexión | 85 MPa Show Supplier Material materials with Resistencia a la flexión of 85 MPa | ISO 178 | 2 mm/min | |
Resistencia al choque, ensayo Izod entallado | -40 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 30 kJ/m² | ISO 180-1A | |
-30 °C | 39 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 39 kJ/m² | ISO 180-1A | ||
23 °C | 53 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 53 kJ/m² | ISO 180-1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 7.7e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.7e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
8.1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.1e-05 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | |||||
Temperatura de flexión bajo carga | 104 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 104 °C | ISO 75-1/2 | 1.8 MPa | ||||
123 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 123 °C | ISO 75-1/2 | 0.45 MPa | |||||
Temperatura de reblandecimiento Vicat | 128 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 128 °C | ISO 306 | B50 | 50°C/h | ||||
130 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 130 °C | ISO 306 | B120 | 120°C/h | |||||
Inflamabilidad | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (150x105x1 mm): < 80 mm/min according to ISO 3795 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.65 - 0.75 % Show Supplier Material materials with Contracción of 0.65 - 0.75 % | ISO 294-4 | 60x60x2 mm |
0.65 - 0.75 % Show Supplier Material materials with Contracción of 0.65 - 0.75 % | ISO 294-4 | 60x60x2 mm, Transverse | |
Velocidad de flujo del volumen derretido | 21 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 21 cm³/10min | ISO 1133 | 260°C/5Kg |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Chemical composition | Thermoplastic polymer blend based on polycarbonate (PC) and acrylonitrile-butadiene-styrene (ABS). | |
Color | White to slightly yellowish. | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 260 ºC according to ISO 294 Injection molding-mold temperature: 80 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |