General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Butadiene content | 27 % Show Supplier Material materials with Butadiene content of 27 % | Lab - IR | |
Densidad | 25 °C | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ISO 1183-1 |
Monómero residual | 300 mg/kg Show Supplier Material materials with Monómero residual of 300 mg/kg | Lab - CG |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 5 % Show Supplier Material materials with Elongación of 5 % | ISO 527-1/2 | min. | 50 mm/min | |
Hardness, Ball Indentation | 72 MPa Show Supplier Material materials with Hardness, Ball Indentation of 72 MPa | ISO 2039-1 | ||
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | ISO 527-1/2 | 50 mm/min | |
Módulo de flexión | 1.7 GPa Show Supplier Material materials with Módulo de flexión of 1.7 GPa | ISO 178 | 2 mm/min | |
Módulo elástico | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | ISO 527-1/2 | 1 mm/min | |
Resistencia al choque, ensayo Izod entallado | -30 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 21 kJ/m² | ISO 180-1A | |
23 °C | 28 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 28 kJ/m² | ISO 180-1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | IEC 60695-2-12 | 2.0 mm | ||
Temperatura de reblandecimiento Vicat | 93 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 93 °C | ISO 306 | B50 | 50°C/h | ||
Inflamabilidad | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (150x105x1 mm): 60 mm/min according to ISO 3795 |
Óptico
Property | Value | Testing Standard |
---|---|---|
Yellowness Index | 31 [-] Show Supplier Material materials with Yellowness Index of 31 [-] | E313 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo del volumen derretido | 14 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 14 cm³/10min | ISO 1133 | 220°C/10Kg |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |