General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Densidad | 25 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183-1 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 27 % Show Supplier Material materials with Elongación of 27 % | ISO 527-1/2 | 50 mm/min | |
Hardness, Ball Indentation | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | ||
Límite elástico | 43 MPa Show Supplier Material materials with Límite elástico of 43 MPa | ISO 527-1/2 | 50 mm/min | |
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 527-1/2 | 2 mm/min | |
Módulo elástico | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | ISO 527-1/2 | 1 mm/min | |
Resistencia a la flexión | 70 MPa Show Supplier Material materials with Resistencia a la flexión of 70 MPa | ISO 178 | 2 mm/min | |
Resistencia al choque, ensayo Izod entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180-1A | |
23 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 21 kJ/m² | ISO 180-1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
Temperatura de flexión bajo carga | 100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 100 °C | ISO 75-1/2 | 1.8 MPa | ||||
104 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 104 °C | ISO 75-1/2 | 0.45 MPa | |||||
Temperatura de reblandecimiento Vicat | 103 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 103 °C | ISO 306 | B50 | 50°C/h | ||||
Inflamabilidad | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (200x105x2 mm): < 55 mm/min according to ISO 3795 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.6 - 0.7 % Show Supplier Material materials with Contracción of 0.6 - 0.7 % | ISO 294-4 | 60x60x2 mm |
0.6 - 0.7 % Show Supplier Material materials with Contracción of 0.6 - 0.7 % | ISO 294-4 | 60x60x2 mm, Transverse | |
Velocidad de flujo del volumen derretido | 22 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 22 cm³/10min | ISO 1133 | 220°C/10Kg |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Color | White to slightly yellowish. | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |