General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Densidad | 25 °C | 1.05 g/cm³ Show Supplier Material materials with Densidad of 1.05 g/cm³ | ISO 1183-1 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Hardness, Ball Indentation | 103 MPa Show Supplier Material materials with Hardness, Ball Indentation of 103 MPa | ISO 2039-1 | ||
Límite elástico | 41 MPa Show Supplier Material materials with Límite elástico of 41 MPa | ISO 527-1/2 | 50 mm/min | |
Módulo de flexión | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ISO 527-1/2 | 2 mm/min | |
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO 527-1/2 | 1 mm/min | |
Resistencia a la flexión | 65 MPa Show Supplier Material materials with Resistencia a la flexión of 65 MPa | ISO 178 | 2 mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179-1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18 kJ/m² | ISO 179-1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | ISO 179-1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | ISO 179-1eU | ||
Resistencia al choque, ensayo Izod entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180-1A | |
23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 18 kJ/m² | ISO 180-1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0001 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0001 1/K | ISO 11359-1/2 | 23 to 55°C | |
0.0001 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0001 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | ||
Temperatura de flexión bajo carga | 92 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 92 °C | ISO 75-1/2 | 1.8 MPa | |
97 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 97 °C | ISO 75-1/2 | 0.45 MPa | ||
Temperatura de reblandecimiento Vicat | 95 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 95 °C | ISO 306 | 50 N | 50°C/h | |
97 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 97 °C | ISO 306 | 50 N | 120°C/h |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 2.9 [-] Show Supplier Material materials with Constante dieléctrica of 2.9 [-] | 100Hz | IEC 60250 | |
2.9 [-] Show Supplier Material materials with Constante dieléctrica of 2.9 [-] | 1MHz | IEC 60250 | ||
Factor de disipación | 0.0073 [-] Show Supplier Material materials with Factor de disipación of 0.0073 [-] | 100Hz | IEC 60250 | |
0.009 [-] Show Supplier Material materials with Factor de disipación of 0.009 [-] | 1MHz | IEC 60250 | ||
Rigidez dieléctrica | 35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | IEC 60243-1 | 1 mm | |
Surface resistivity | 1e+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+16 Ω/sq | |||
Volume resistivity | 1e+18 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+18 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.6 % Show Supplier Material materials with Contracción of 0.6 % | ISO 2577 | 150x105x3 |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | ISO 2577 | 150x105x3, Transverse | |
Velocidad de flujo del volumen derretido | 32 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 32 cm³/10min | ISO 1133 | 220°C/10Kg |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 80 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |