General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Absorción de agua | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | DIN EN ISO 62 | max. | 23°C | 50 % r.h. up to saturation |
Densidad | 1.59 g/cm³ Show Supplier Material materials with Densidad of 1.59 g/cm³ |
Mecánica
Property | Value | Testing Standard |
---|---|---|
Elongación | 1 % Show Supplier Material materials with Elongación of 1 % | DIN EN ISO 527-1 |
Módulo elástico | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | DIN EN ISO 527-1 |
Resistencia a la tracción | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | DIN EN ISO 527-1 |
Resistencia al choque, ensayo Charpy no entallado | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 8 kJ/m² | DIN EN ISO 179-1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Calor específico | 1500 J/(kg·K) Show Supplier Material materials with Calor específico of 1500 J/(kg·K) | DIN EN 821 | |||||
Coeficiente de dilatación térmica | 6.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5e-05 1/K | DIN EN ISO 11359-1/2 | at 23-100°C | ||||
8.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.5e-05 1/K | DIN EN ISO 11359-1/2 | at 23-100°C, Transverse | |||||
Conductividad térmica | 3 W/(m·K) Show Supplier Material materials with Conductividad térmica of 3 W/(m·K) | DIN EN 821 | through-plane | ||||
11.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 11.5 W/(m·K) | DIN EN 821 | in-plane | |||||
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | ISO-R 75 Method A | 1.8 MPa | ||||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | DIN 53765 | |||||
Temperatura de transición del vidrio | 60 °C Show Supplier Material materials with Temperatura de transición del vidrio of 60 °C | DIN 53765 | |||||
Temperatura máx. de funcionamiento | 110 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 110 °C | Long | |||||
170 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 170 °C | Short | ||||||
Inflamabilidad | UL94 class HB, DIN IEC 60695-11-10 |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 10000 Ω/sq Show Supplier Material materials with Surface resistivity of 10000 Ω/sq | DIN EN 61340-2-3 | max. |
Volume resistivity | 1e+06 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+06 Ω·cm | DIN EN 61340-2-3 | max. |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.8 % Show Supplier Material materials with Contracción of 0.8 % | DIN EN ISO 294-4 | |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | DIN EN ISO 294-4 | Transverse | |
Velocidad de flujo de la masa derretida | 19 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 19 g/10min | DIN EN ISO 1133 | 280°C/5kg |
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | DIN EN ISO 1133 | 280°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical engineering , Mechanical engineering , Automotive industry camera, moulded interconnect device (PCB, LDS), power distribution in electronics and radar | |
Color | Black | |
Fillers | Graphite | |
Processing methods | Permissible residual moisture content (%): 0.02, drying temperature (°C): 120, drying time (h): 6, mould temperature (°C): 130, material temperature (°C): 280, cylinder/processing temperature (°C): 270 |