General
Property | Value |
---|---|
Densidad | 1.42 g/cm³ Show Supplier Material materials with Densidad of 1.42 g/cm³ |
Mecánica
Property | Value | Testing Standard |
---|---|---|
Elongación | 9.5 % Show Supplier Material materials with Elongación of 9.5 % | DIN EN ISO 527-1 |
Módulo elástico | 1.1 GPa Show Supplier Material materials with Módulo elástico of 1.1 GPa | DIN EN ISO 527-1 |
Resistencia a la tracción | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | DIN EN ISO 527-1 |
Resistencia al choque, ensayo Charpy no entallado | 28 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 28 kJ/m² | DIN EN ISO 179-1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 109 °C Show Supplier Material materials with Temperatura de fusión of 109 °C | ||
Temperatura de transición del vidrio | -100 °C Show Supplier Material materials with Temperatura de transición del vidrio of -100 °C | DIN 53765 | |
Temperatura máx. de funcionamiento | 70 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 70 °C | Long | |
100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Short |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.9 % Show Supplier Material materials with Contracción of 1.9 % | DIN EN ISO 294-4 | |
3.5 % Show Supplier Material materials with Contracción of 3.5 % | DIN EN ISO 294-4 | Transverse | |
Velocidad de flujo de la masa derretida | 11 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 11 g/10min | DIN EN ISO 1133 | 230°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Certifications | Explanation of food contact according to FDA and EU 10/2011 on request | |
Color | Blue | |
Detectability | Inductive: 6 mm Al | |
Fillers | Mineral Powder | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 4, mould temperature (°C): 60, material temperature (°C): 240, cylinder/processing temperature (°C): 240 |