General
Property | Value |
---|---|
Densidad | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell C | 57 - 60 [-] Show Supplier Material materials with Dureza Rockwell C of 57 - 60 [-] | |
Dureza Vickers | 815 - 905 [-] Show Supplier Material materials with Dureza Vickers of 815 - 905 [-] | HV 0.2 |
Resistencia a la tracción | 1000-1300 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Mechanics | |
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks. 20 x 10 x 2 to 6 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |