General
Property | Value |
---|---|
Densidad | 8.7 g/cm³ Show Supplier Material materials with Densidad of 8.7 g/cm³ |
Mecánica
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |