General
Property | Value |
---|---|
Densidad | 10.26 g/cm³ Show Supplier Material materials with Densidad of 10.26 g/cm³ |
Porosidad | 1 % Show Supplier Material materials with Porosidad of 1 % |
Mecánica
Property | Value |
---|---|
Dureza Vickers | 92 - 109 [-] Show Supplier Material materials with Dureza Vickers of 92 - 109 [-] |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 3.63e-08 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.63e-08 Ω·m |
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-5 mm disks. Diameter 15 mm by 2-5 mm disks Special shapes upon request. | |
Processing methods | E-Forged™ from powders |