General
Property | Value |
---|---|
Densidad | 2.47 g/cm³ Show Supplier Material materials with Densidad of 2.47 g/cm³ |
Porosidad | 1 % Show Supplier Material materials with Porosidad of 1 % |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 1.06e-05 - 1.23e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.06e-05 - 1.23e-05 1/K |
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks. 20 x 10 x 2 to 6 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |