General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Densidad of 1.42 g/cm³ | ISO 1183 |
Water content | 23.0 °C | 0.1 % Show Supplier Material materials with Water content of 0.1 % | ISO 15512 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527-2 (5mm/min) |
Hardness, Ball Indentation | 23.0 °C | 240 MPa Show Supplier Material materials with Hardness, Ball Indentation of 240 MPa | ISO 2039-1 |
Módulo elástico | 23.0 °C | 11.4 GPa Show Supplier Material materials with Módulo elástico of 11.4 GPa | ISO 527-2 (1mm/min) |
Resistencia a la tracción | 23.0 °C | 190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | ISO 527-2 (5mm/min) |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA |
23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 30 % Show Supplier Material materials with Contenido de cenizas of 30 % | ISO 3451-4 | ||
Heat deflection temperature, 1.80 MPa | 280 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 280 °C | ISO 75-2/A | |||
Heat deflection temperature, 8.0 MPa | 150 °C Show Supplier Material materials with Heat deflection temperature, 8.0 MPa of 150 °C | ISO 75-2/B | |||
Temperatura de fusión | 310 °C Show Supplier Material materials with Temperatura de fusión of 310 °C | ISO 3146 | |||
Temperatura máx. de funcionamiento, corto | 250 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, corto of 250 °C | ISO 2578 | |||
Temperatura máx. de funcionamiento, largo | 140 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, largo of 140 °C | ISO 2578 | |||
Inflamabilidad | UL94 (0.8mm) HB |
Eléctrico
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Eplamid HT02 grades are used for molding technical parts where higher operating temperatures and higher stiffness in moist environments are required. | |
Fillers | 30% Glass Fiber | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |