Heat deflection temperature, 8.0 MPa: 150 °C

Quick Comparison

Copolyamide 6T/66 (PA6T/66)

Polyphthalamide (PPA) HT02 GFR 20 BK Q1C001

Suministrada por:

EPSAN

Copolyamide 6T/66 (PA6T/66)

Polyphthalamide (PPA) HT02 GFR 30 BK Q1D001

Suministrada por:

EPSAN

Copolyamide 6T/66 (PA6T/66)

Polyphthalamide (PPA) HT02 GFR 45 BK Q1E501

Suministrada por:

EPSAN

Copolyamide 6T/66 (PA6T/66)

Polyphthalamide (PPA) HT02 GFR 50 BK Q1F001

Suministrada por:

EPSAN