General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9 - 10.2 g/cm³ Show Supplier Material materials with Densidad of 9 - 10.2 g/cm³ | (depends on the forming degree) |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 5 - 20 % Show Supplier Material materials with Elongación of 5 - 20 % |
Resistencia a la tracción | 23.0 °C | 500 - 1000 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 1000 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4.8E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.8E-6 1/K | at 0–100°C |
Conductividad térmica | 23.0 °C | 142 W/(m·K) Show Supplier Material materials with Conductividad térmica of 142 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 27.0 °C | 5.5E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.5E-6 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 2E-3 % Show Supplier Material materials with Aluminio of 2E-3 % | Max. |
Arsénico | 2E-3 % Show Supplier Material materials with Arsénico of 2E-3 % | Max. |
Azufre | 2E-3 % Show Supplier Material materials with Azufre of 2E-3 % | Max. |
Calcio | 2E-3 % Show Supplier Material materials with Calcio of 2E-3 % | Max. |
Carbono | 5E-3 % Show Supplier Material materials with Carbono of 5E-3 % | Max. |
Cobalto | 3E-3 % Show Supplier Material materials with Cobalto of 3E-3 % | Max. |
Cobre | 1E-3 % Show Supplier Material materials with Cobre of 1E-3 % | Max. |
Cromo | 2E-3 % Show Supplier Material materials with Cromo of 2E-3 % | Max. |
Hierro | 3E-3 % Show Supplier Material materials with Hierro of 3E-3 % | Max. |
Magnesio | 2E-3 % Show Supplier Material materials with Magnesio of 2E-3 % | Max. |
Molibdeno | 99.9 % Show Supplier Material materials with Molibdeno of 99.9 % | Min. |
Níquel | 2E-3 % Show Supplier Material materials with Níquel of 2E-3 % | Max. |
Potasio | 1E-3 % Show Supplier Material materials with Potasio of 1E-3 % | Max. |
Silicona | 3E-3 % Show Supplier Material materials with Silicona of 3E-3 % | Max. |
Sodio | 2E-3 % Show Supplier Material materials with Sodio of 2E-3 % | Max. |
Wolframio | 0.03 % Show Supplier Material materials with Wolframio of 0.03 % | Max. |
Technological properties
Property | ||
---|---|---|
Application areas | Alloying element for steel; Coating material; Heating element; Mount and current feedthrough for tungsten; Wires in lamps; Targets in x-ray tubes | |
Processing history | Heat treatment: annealed, unannealed | |
Surface Finish | ground, drawn (black/cleaned), hammered |