General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 17.8 - 18.2 g/cm³ Show Supplier Material materials with Densidad of 17.8 - 18.2 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 290 - 340 [-] Show Supplier Material materials with Dureza Vickers 10 of 290 - 340 [-] |
Elongación | 23.0 °C | 3 - 25 % Show Supplier Material materials with Elongación of 3 - 25 % |
Resistencia a la tracción | 23.0 °C | 750 - 950 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 950 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 2E-3 % Show Supplier Material materials with Aluminio of 2E-3 % | Max. | |
Arsénico | 2E-3 % Show Supplier Material materials with Arsénico of 2E-3 % | Max. | |
Azufre | 2E-3 % Show Supplier Material materials with Azufre of 2E-3 % | Max. | |
Calcio | 2E-3 % Show Supplier Material materials with Calcio of 2E-3 % | Max. | |
Carbono | 5E-3 % Show Supplier Material materials with Carbono of 5E-3 % | Max. | |
Cobalto | 3E-3 % Show Supplier Material materials with Cobalto of 3E-3 % | Max. | |
Cobre | 1E-3 % Show Supplier Material materials with Cobre of 1E-3 % | Max. | |
Cromo | 2E-3 % Show Supplier Material materials with Cromo of 2E-3 % | Max. | |
Magnesio | 2E-3 % Show Supplier Material materials with Magnesio of 2E-3 % | Max. | |
Molibdeno | 5E-3 % Show Supplier Material materials with Molibdeno of 5E-3 % | Max. | |
Otro | 5 % Show Supplier Material materials with Otro of 5 % | Ni+Fe | |
Potasio | 1E-3 % Show Supplier Material materials with Potasio of 1E-3 % | Max. | |
Silicona | 3E-3 % Show Supplier Material materials with Silicona of 3E-3 % | Max. | |
Sodio | 2E-3 % Show Supplier Material materials with Sodio of 2E-3 % | Max. | |
Wolframio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | Material to balance rotating systems (aviation, radar, crankshafts etc.); Radiation protection material (Shielding parts for medical diagnostic and radiation therapy); Material for tool holders and high speed spindles; Upsetting tools; Moulds for aluminium, magnesium, zinc and copper high pressure die casting |