Material: el 'Carbon Fibre Tenax HTA Multi Filament Tow' que buscabas ha sido remplazado por el material siguiente.

Carbon Fibre Tenax HTA Multi Filament Tow

Want to keep this datasheet? Save it now in your required format

Description

Continuous multi-filament TOW.


The most common form of carbon fibre is the high strength, high stiffness form commonly used in composites. These are made by a complicated process from textile pre-cursor yarns made from either Polyacrylonitrile (PAN) or pitch that results in a predominantly graphitic structure highly oriented in the direction of the fibre axis. This high orientation gives them their remarkable properties which include a small negative coefficient of thermal expansion in the axial direction as well as remarkably high specific strength and stiffness.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Calibrado

23.0 °C

1.3 %

Show Material materials with Calibrado of 1.3 %

Densidad

23.0 °C

1.76 g/cm³

Show Material materials with Densidad of 1.76 g/cm³

Densidad lineal

23.0 °C

4.00E+7 g/cm

Show Material materials with Densidad lineal of 4.00E+7 g/cm

Número de filamentos

23.0 °C

6000 [-]

Show Material materials with Número de filamentos of 6000 [-]

Tex

23.0 °C

400 [-]

Show Material materials with Tex of 400 [-]

Tipo de fibra

PAN carbon fiber

Medidas

PropertyValueComment

Ancho

2.13 mm

Show Material materials with Ancho of 2.13 mm

Diámetro

7E-3 mm

Show Material materials with Diámetro of 7E-3 mm

filament diameter

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

23.0 °C

0.29 [-]

Show Material materials with Coeficiente de Poisson of 0.29 [-]

Elongación

23.0 °C

1.7 %

Show Material materials with Elongación of 1.7 %

Módulo elástico

23.0 °C

238 GPa

Show Material materials with Módulo elástico of 238 GPa

Resistencia a la tracción

23.0 °C

3950 MPa

Show Material materials with Resistencia a la tracción of 3950 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

23.0 °C

710 J/(kg·K)

Show Material materials with Calor específico of 710 J/(kg·K)

Coeficiente de dilatación térmica

23.0 °C

-1E-7 1/K

Show Material materials with Coeficiente de dilatación térmica of -1E-7 1/K

Conductividad térmica

23.0 °C

17 W/(m·K)

Show Material materials with Conductividad térmica of 17 W/(m·K)

Eléctrico

PropertyTemperatureValue

Resistividad eléctrica

23.0 °C

1.6E-5 Ω·m

Show Material materials with Resistividad eléctrica of 1.6E-5 Ω·m

Technological properties

Property
Processing history

Epoxy sized 1.2%