Property | Value | Comment |
---|---|---|
Bio-based content | 28.0 % Show Supplier Material materials with Bio-based content of 28.0 % | |
Densidad | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 83.0 [-] Show Supplier Material materials with Dureza Shore A of 83.0 [-] | ASTM D2240 |
Elongación | 750.0 % Show Supplier Material materials with Elongación of 750.0 % | ASTM D412 |
Resistencia a desgarros | 115.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 115.0 kN/m | ASTM D624 |
Resistencia a la tracción | 23.0 MPa Show Supplier Material materials with Resistencia a la tracción of 23.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |