Bio-based content: 28 %

Quick Comparison

Poliamida termoplástica

Pebax® Rnew® 35R53 SP 01

Suministrada por:

Arkema: High Performance Polymers

Poliuretano termoplástico (TPU)

TPU G1085AEU-J2

Suministrada por:

Great Eastern Resins Industrial Co. Ltd.

Poliuretano termoplástico (TPU)

TPU G1085AU-L

Suministrada por:

Great Eastern Resins Industrial Co. Ltd.