General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.94 g/cm³ Show Supplier Material materials with Densidad of 0.94 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 55 [-] Show Supplier Material materials with Dureza Shore D of 55 [-] | ASTM D2240 |
Elongación | 23.0 °C | 165 - 600 % Show Supplier Material materials with Elongación of 165 - 600 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 250 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250 J/m | ASTM D256 |
Límite elástico | 23.0 °C | 17.5 - 18 MPa Show Supplier Material materials with Límite elástico of 17.5 - 18 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 0.23 - 0.59 GPa Show Supplier Material materials with Módulo de flexión of 0.23 - 0.59 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 11.75 MPa Show Supplier Material materials with Resistencia a la tracción of 11.75 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 117 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 117 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 4.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4.5 g/10min | ASTM D1238, 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3645UV is suggested for the production of wide variety of Storage tank applications of water, chemicals & Oils. GREENETHENE G-3645UV can also be used for off-shore flotation buoys and road crash barriers. | |
Certifications | List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996 | |
Color | Natural, black, terracotta, fire red, yellow and blue. | |
Processing methods | Compression molded & rotomolded |