General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Supplier Material materials with Densidad of 0.92 g/cm³ | ASTM D792 |
Moisture absorption | 23.0 °C | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ASTM D6982, 100°C - 1hr |
Mecánica
Technological properties
Property | ||
---|---|---|
Application areas | Electric Hoses - Film Grades | |
Color | Honey |