General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.9 g/cm³ Show Supplier Material materials with Densidad of 0.9 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Hardness, Rockwell R | 23.0 °C | 75 [-] Show Supplier Material materials with Hardness, Rockwell R of 75 [-] | ASTM D785 |
Impact strength, Izod unnotched, ASTM | -10.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m | ASTM D256 |
Límite elástico | 23.0 °C | 26.48 MPa Show Supplier Material materials with Límite elástico of 26.48 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 0.88 GPa Show Supplier Material materials with Módulo de flexión of 0.88 GPa | ASTM D790 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 80.0 °C | 1.5E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5E-4 1/K | Mean value between 0°C and the mentioned temperature, Dilatometer |
Heat deflection temperature, 0.45 MPa | 90 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 90 °C | ASTM D648 | |
Temperatura de fusión | 141 °C Show Supplier Material materials with Temperatura de fusión of 141 °C | ASTM D3418 | |
Temperatura de reblandecimiento Vicat | 130 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 130 °C | ASTM D1525 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | Minimum, ASTM HS Method |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0.25 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 0.25 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Pipes and fittings, piping for house, radiator pipes, idustrial pipes |