General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Hardness, Rockwell R | 23.0 °C | 85 [-] Show Supplier Material materials with Hardness, Rockwell R of 85 [-] | ASTM D785 |
Impact strength, Izod unnotched, ASTM | -10.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m | ASTM D256 |
23.0 °C | 140 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 140 J/m | ASTM D256 | |
Límite elástico | 23.0 °C | 41.19 MPa Show Supplier Material materials with Límite elástico of 41.19 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 1.96 GPa Show Supplier Material materials with Módulo de flexión of 1.96 GPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ASTM D648 |
Temperatura de fusión | 143 °C Show Supplier Material materials with Temperatura de fusión of 143 °C | ASTM D3418 |
Temperatura de reblandecimiento Vicat | 135 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 135 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0.3 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 0.3 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Pipes and fittings, piping for house, radiator pipes, idustrial pipes | |
Fillers | 20% Glass Fiber |