It is a CuCrZr alloy that can be hardened by cold forming and by precipitation of CuCrZr - phases during a heat treatment. It has good bendability, excellent hot and cold forming properties, a high strength and a good corrosion resistance. Due to the CrZr-precipitations the relaxation properties, even at temperatures up to 250°C are excellent. The electrical and thermal conductivity is excellent. Welding, soldering and brazing properties are good too. The alloy is registered in the US by EPA to have good antimicrobial properties.

Equivalent Materials

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

8.9 g/cm³

Show Material materials with Densidad of 8.9 g/cm³

Mecánica

PropertyTemperatureValueComment

Dureza Vickers

23.0 °C

150 - 190 [-]

Show Material materials with Dureza Vickers of 150 - 190 [-]

Elongación A50

23.0 °C

8 %

Show Material materials with Elongación A50 of 8 %

Límite elástico Rp 0,2

23.0 °C

450 MPa

Show Material materials with Límite elástico Rp 0,2 of 450 MPa

Módulo elástico

23.0 °C

137 GPa

Show Material materials with Módulo elástico of 137 GPa

cold formed

Plegabilidad 180 ° bidireccional

23.0 °C

2 [-]

Show Material materials with Plegabilidad 180 ° bidireccional of 2 [-]

r = x t, t <0.5mm

Plegabilidad 180 ° en peso bruto

23.0 °C

2 [-]

Show Material materials with Plegabilidad 180 ° en peso bruto of 2 [-]

r = x t, t <0.5mm

Plegabilidad 90 ° bidireccional

23.0 °C

1.5 [-]

Show Material materials with Plegabilidad 90 ° bidireccional of 1.5 [-]

r = x t, t <0.5mm

Plegabilidad 90 ° en peso bruto

23.0 °C

1.5 [-]

Show Material materials with Plegabilidad 90 ° en peso bruto of 1.5 [-]

r = x t, t <0.5mm

Resistencia a la tracción

23.0 °C

480 - 560 MPa

Show Material materials with Resistencia a la tracción of 480 - 560 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

381 J/(kg·K)

Show Material materials with Calor específico of 381 J/(kg·K)

Coeficiente de dilatación térmica

300.0 °C

1.8E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K

for 20°C to the mentioned temperature

Conductividad térmica

23.0 °C

330 W/(m·K)

Show Material materials with Conductividad térmica of 330 W/(m·K)

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

23.0 °C

5.00E+7 - 5.30E+7 S/m

Show Material materials with Conductividad eléctrica of 5.00E+7 - 5.30E+7 S/m

Specific Electrical conductivity

86 % IACS

Show Material materials with Specific Electrical conductivity of 86 % IACS

Chemical properties

PropertyValueComment

Circonio

0.05 - 0.25 %

Show Material materials with Circonio of 0.05 - 0.25 %

Cobre

Balance

Cromo

0.2 - 1.2 %

Show Material materials with Cromo of 0.2 - 1.2 %

Hierro

0.1 %

Show Material materials with Hierro of 0.1 %

max.

Silicona

0.1 %

Show Material materials with Silicona of 0.1 %

max.

Technological properties

Property
Application areas

Automotive: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Hybrid Cars. Electrical: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Components for the electrical industry, Stamped parts, Semiconductor Components, Junction Boxes, Photovoltaic Systems.

Brazing

Excellent

Cold Forming

Good

Corrosion properties

STOL® 95 is resistant to pure water vapour and non oxidizingacids and alkalis as well as neutral saline solutions. The material is insensitive to stress corrosion cracking.

Heat Treatment

Temper: R480

Machining

Rating 20, less suitable

Other

This alloy is in accordance with RoHS 2002/96/CE for electric & electronic equipments and 2002/53/CE for automotive industry. It is suitable for high voltage applications as hybrid cars or photovoltaics.

Plating

Electroplating is excellent

Welding

Gas Shielded Arc Welding: Excellent, Laser Welding: Fair

Looking for suppliers of this material? Click to see 2 supplier of STOL® 95 R480 on Matmatch