General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.5 - 2.5 % Show Supplier Material materials with Elongación of 1.5 - 2.5 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 267 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 267 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 908 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 908 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 8.27 GPa Show Supplier Material materials with Módulo de flexión of 8.27 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 8.96 GPa Show Supplier Material materials with Módulo elástico of 8.96 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la flexión of 179 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 121 MPa Show Supplier Material materials with Resistencia a la tracción of 121 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Contracción of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Car front and back module, Water tank frame, Battery bracket, Engine cover, Skylight frame | |
Color | Natural | |
Fillers | 40% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C |