General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 - 3 % Show Supplier Material materials with Elongación of 2 - 3 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 267 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 267 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1175 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1175 J/m | ASTM D4812 |
Módulo de flexión | 23.0 °C | 6.21 GPa Show Supplier Material materials with Módulo de flexión of 6.21 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 221 MPa Show Supplier Material materials with Resistencia a la flexión of 221 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D648 | |
Inflamabilidad | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.2 % Show Supplier Material materials with Contracción of 0.1 - 0.2 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Car Doors and window, Mechanical parts, Pneumatic nail gun boxes, Nut and bolts, Fireman shoe parts (safety shoe parts) | |
Color | Black/white or custom color | |
Fillers | 20% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 221 - 243 °C, Mould temperature 52 - 93 °C, Pre-drying 6 hrs @ 107 °C, Moisture Content 0.01%, Dew Point -40°C |