General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Calibrado | 3 % Show Supplier Material materials with Calibrado of 3 % | ASTM D1921 | max. | #10 mesh on |
Densidad aparente | 0.25 g/cm³ Show Supplier Material materials with Densidad aparente of 0.25 g/cm³ | ASTM D1895 | min. | aerated |
Foreign material | 3 [-] Show Supplier Material materials with Foreign material of 3 [-] | LSY QB KD005 (LG test) | max. |
Volatile share | 1 % Show Supplier Material materials with Volatile share of 1 % | ISO 1625 | max. |
Mecánica
Property | Temperature | Value | Thickness | Testing Standard |
---|---|---|---|---|
Impact strength, Izod unnotched, ASTM | -30 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 100 J/m | 6.35 mm | ASTM D256 |
-30 °C | 400 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 400 J/m | 3 mm | ASTM D256 | |
23 °C | 500 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 500 J/m | 6.35 mm | ASTM D256 | |
23 °C | 600 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 600 J/m | 3 mm | ASTM D256 |
Technological properties
Property | ||
---|---|---|
Application areas | Impact modifier for engineering plastics, PC Alloy (PC, PC/ABS, PC/PBT) etc | |
Other | Before using this product, consult the Safety Data sheet(SDS) for details on product hazards, recommended handling the precautions and product storage. FIFO: LG products should be consumed in First in, First out Rule Customer notice: LG strongly encourages its customers to use products in qualified and tested applications. If customers use our product in new application or changing formulation, LG personnel are available to provide reasonable technical support. LG product technical reports including SDS, TDS etc, should be consulted prior to sue of LG products. Combustible flammable: Keep combustible and/or flammable products and their vapors away from heat, sparks, flames and other sources of ignition including static discharge. Use appropriate grounding and bonding techniques to manage static discharge hazards. Dust explosion: Avoid high concentrations of dust in air and accumulation of dust on equipment. An airborne dust of this material can create a dust explosion. To prevent dust explosions, employ bonding and grounding for operations capable of generating static electricity. Carrying Processing: When carrying and processing this material, local ventilation may be required to control dust and reduce exposure to vapors. Shelf Life: Before using the product, check shelf life in COA. If you can’t find it, contact proper persons. Storage conditions: Store ambient temperature/atmospheric pressure and a well ventilated areas Keep away from direct sunlight, Store in product in roofed and ventilated warehouse Keep container closed when not in use Do not stack Flecon bag over double stack to prevent lumps of product. |