General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 0.94 g/cm³ Show Supplier Material materials with Densidad of 0.94 g/cm³ | ISO 2781 | typical value |
Styrene content | 31 % Show Supplier Material materials with Styrene content of 31 % | LSY-QB-SD0151 (LG test) | typical value |
Volatile share | 0.6 % Show Supplier Material materials with Volatile share of 0.6 % | ASTM D1416 | max. |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 84 [-] Show Supplier Material materials with Dureza Shore A of 84 [-] | ASTM D2240 | typical value |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Yellowness Index | 6 [-] Show Supplier Material materials with Yellowness Index of 6 [-] | ASTM D1925 | max. |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Kinematic viscosity | 28.4 cSt Show Supplier Material materials with Kinematic viscosity of 28.4 cSt | ASTM D445 | typical value | Toluene Solution Viscosity 5% |
Technological properties
Property | ||
---|---|---|
Application areas | Asphalt Modifier, Plastic Modifier Compounding, Adhesives, etc | |
Other | Physical Form: Porous pellet(LG411S), Powder(LG411W) Packaging: Paper bag(20kg), Flecon bag(500kg) |