General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.91 g/cm³ Show Supplier Material materials with Densidad of 8.91 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 0.04 - 0.5 mm Show Supplier Material materials with Espesor of 0.04 - 0.5 mm | gauge |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-] | |
Dureza Vickers | 23.0 °C | 240 - 360 [-] Show Supplier Material materials with Dureza Vickers of 240 - 360 [-] | |
Elongación | 23.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | for strip thicker than 0.10 mm |
Límite elástico Rp 0,2 | 23.0 °C | 621 - 896 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 621 - 896 MPa | |
Módulo elástico | 23.0 °C | 124 GPa Show Supplier Material materials with Módulo elástico of 124 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 3 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 3 [-] | |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 2.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 2.5 [-] | |
Resistencia a la tracción | 23.0 °C | 827 - 965 MPa Show Supplier Material materials with Resistencia a la tracción of 827 - 965 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.80E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.80E+6 S/m |
Specific Electrical conductivity | 10 % IACS Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.01 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.01 [-] | max. |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Estaño | 5.5 - 6.5 % Show Supplier Material materials with Estaño of 5.5 - 6.5 % |
Níquel | 8.5 - 9.5 % Show Supplier Material materials with Níquel of 8.5 - 9.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic connectors, Switches & Sensors |