Specific Electrical conductivity: 10 % IACS

Quick Comparison

Bronce fosforado

UNS C52400 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51000 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

JIS C5240HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Nickel Grade

BrushForm® 96 TB00 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD01 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD04 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM00 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM02 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM04 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM06 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD02 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM08 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Bronce fosforado

JIS C5240 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Bronze Aluminium Bronze

AMPCO® 21 Extruded and drawn rounds and rectangular bars

Suministrada por:

AMPCO METAL

Wrought Copper Nickel Grade

BrushForm® 96 TX00 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TS01 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TS02 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TS04 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Cast Copper Bronze Aluminium Bronze

AMPCO® 21 Centrifugal castings

Suministrada por:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 21 Sand castings

Suministrada por:

AMPCO METAL
Página 1 de 3