General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Densidad of 8.83 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 23.0 °C | 97 [-] Show Supplier Material materials with Dureza Rockwell B of 97 [-] |
Dureza Rockwell C | 23.0 °C | 20 [-] Show Supplier Material materials with Dureza Rockwell C of 20 [-] |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % |
Energía de impacto Charpy | 23.0 °C | 55 J Show Supplier Material materials with Energía de impacto Charpy of 55 J |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 620 MPa |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa |
Resistencia a la tracción | 23.0 °C | 725 MPa Show Supplier Material materials with Resistencia a la tracción of 725 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 100.0 °C | 410 J/(kg·K) Show Supplier Material materials with Calor específico of 410 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K |
Conductividad térmica | 100.0 °C | 250 W/(m·K) Show Supplier Material materials with Conductividad térmica of 250 W/(m·K) |
Temperatura de fusión | 1040 °C Show Supplier Material materials with Temperatura de fusión of 1040 °C |
Chemical properties
Property | Value |
---|---|
Berilio | 0.2 - 0.6 % Show Supplier Material materials with Berilio of 0.2 - 0.6 % |
Cobre | Balance |
Níquel | 1.4 - 2.2 % Show Supplier Material materials with Níquel of 1.4 - 2.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | PROtherm alloy is used as blow mold cavities, injection mold cores and cavities and hot runners. |