Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH042000 Serie
EN 573-3 Grade AW-2014A T42000 Serie
EN 573-3 Grade AW-2014A T42000 Serie
EN 573-3 Grade AW-2014A T62000 Serie
EN 573-3 Grade AW-2014A T62000 Serie
EN 573-3 Grade AW-2014A O2000 Serie
EN 573-3 Grade AW-2014A O2000 Serie
EN 573-3 Grade AW-2014A T4512000 Serie
EN 573-3 Grade AW-2014A T4512000 Serie
EN 573-3 Grade AW-2014A T6512000 Serie
EN 573-3 Grade AW-2014A T6512000 Serie
WL 3.1254-1 Grade 3.1254 T62000 Serie
EN 573-3 Grade AW-2618A T8512000 Serie
WL 3.1254-1 Grade 3.1254 T6112000 Serie
WL 3.1254-1 Grade 3.1254 T6522000 Serie
WL 3.1924-1 Grade 3.1924 T6512000 Serie
EN 573-3 Grade AW-2030 T42000 Serie
EN 573-3 Grade AW-2030 T32000 Serie
EN 573-3 Grade AW-2030 T4