General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.5 - 3.2 g/cm³ Show Material materials with Densidad of 2.5 - 3.2 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.21 - 0.23 [-] Show Material materials with Coeficiente de Poisson of 0.21 - 0.23 [-] |
Dureza Knoop HK2 | 20.0 °C | 450 - 590 [-] Show Material materials with Dureza Knoop HK2 of 450 - 590 [-] |
Módulo elástico | 20.0 °C | 60 - 80 GPa Show Material materials with Módulo elástico of 60 - 80 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 0.66 - 0.82 J/(kg·K) Show Material materials with Calor específico of 0.66 - 0.82 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 7.9E-6 - 1.06E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.9E-6 - 1.06E-5 1/K | from 100 to 300°C |
Conductividad térmica | 20.0 °C | 0.9 - 1.2 W/(m·K) Show Material materials with Conductividad térmica of 0.9 - 1.2 W/(m·K) | |
Temperatura de transición del vidrio | 420 - 590 °C Show Material materials with Temperatura de transición del vidrio of 420 - 590 °C |
Óptico
Property | Value |
---|---|
Número de Abbe | 40.85 - 42.84 [-] Show Material materials with Número de Abbe of 40.85 - 42.84 [-] |
Índice de refracción | 1.57 - 1.58 [-] Show Material materials with Índice de refracción of 1.57 - 1.58 [-] |