General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.5 - 2.6 g/cm³ Show Material materials with Densidad of 2.5 - 2.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.19 - 0.23 [-] Show Material materials with Coeficiente de Poisson of 0.19 - 0.23 [-] |
Dureza Knoop HK2 | 20.0 °C | 450 - 590 [-] Show Material materials with Dureza Knoop HK2 of 450 - 590 [-] |
Módulo elástico | 20.0 °C | 70 GPa Show Material materials with Módulo elástico of 70 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 0.73 - 0.78 J/(kg·K) Show Material materials with Calor específico of 0.73 - 0.78 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 7.4E-6 - 1.22E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.4E-6 - 1.22E-5 1/K | from 100 to 300°C |
Conductividad térmica | 20.0 °C | 0.95 - 1.13 W/(m·K) Show Material materials with Conductividad térmica of 0.95 - 1.13 W/(m·K) | |
Temperatura de transición del vidrio | 460 - 560 °C Show Material materials with Temperatura de transición del vidrio of 460 - 560 °C |
Óptico
Property | Value |
---|---|
Número de Abbe | 56.41 - 60.41 [-] Show Material materials with Número de Abbe of 56.41 - 60.41 [-] |
Índice de refracción | 1.5 - 1.52 [-] Show Material materials with Índice de refracción of 1.5 - 1.52 [-] |